Description
The heat aging characteristics of ethylene propylene rubber (EPR) and the electrical characteristics of polymers are discussed. The EPDM formulation, accelerator cost per 100 lbs, tensile and elongation measurements after curing, aging temperature effects in days and months, and dielectric strength tests are considered.