EPDM endurance promises developing market

$15.00

The heat aging characteristics of ethylene propylene rubber (EPR) and the electrical characteristics of polymers are discussed. The EPDM formulation, accelerator cost per 100 lbs, tensile and elongation measurements after curing, aging temperature effects in days and months, and dielectric strength tests are considered.

SKU: P02759 Category: Tags: ,

Description

The heat aging characteristics of ethylene propylene rubber (EPR) and the electrical characteristics of polymers are discussed. The EPDM formulation, accelerator cost per 100 lbs, tensile and elongation measurements after curing, aging temperature effects in days and months, and dielectric strength tests are considered.

Additional information

Author(s)

McCarthy, J.J.Uniroyal Chemical Div., Mastromatteo, R.P.Mitchell, J.M.

Publication/Event/Pages

Wire Journal3(10): 121-128 1970, Paper presented at WAI Electrical Divisional Meeting, Providence, RI USA

Year

1970