Investigation of wire breaks in aluminum

$15.00

Wire breaks in aluminum wire are reviewed and classified according to cause of failure (material or processing). Material defects considered include inclusions, macroporosity, surface defects, overfills, laps, and slivers. Processing defects include tensile fracture, drawn-in inclusion, galling, and weld failure.

SKU: P03068 Category: Tags: , ,

Description

Wire breaks in aluminum wire are reviewed and classified according to cause of failure (material or processing). Material defects considered include inclusions, macroporosity, surface defects, overfills, laps, and slivers. Processing defects include tensile fracture, drawn-in inclusion, galling, and weld failure.

Additional information

Author(s)

Chia, E.H.Southwire Co., Weber, J.G.Cofer, D.B.

Publication/Event/Pages

Wire Journal9(12): 46-53 1976, Paper presented at WAI Nonferrous/Electrical Divisional Meeting, Toronto, Canada

Year

1976