Progressive work-hardening and reannealing of five brands of high conductivity copper

$15.00

Results are presented of tests carried out to determine the work hardening and reannealing cycles of five brands of high conductivity copper. Data are presented both in tabular form and as space diagrams, relating temperatures and percent cold working to tensile strength and elongation.

Description

Results are presented of tests carried out to determine the work hardening and reannealing cycles of five brands of high conductivity copper. Data are presented both in tabular form and as space diagrams, relating temperatures and percent cold working to tensile strength and elongation.

Additional information

Author(s)

Yokelson, M.V.General Cable Corp., Polytechnic Institute of Brooklyn, Balicki, M., American Smelting & Refining Co.

Publication/Event/Pages

Wire & Wire Products30(10): 1179, 1182-1194, 1285-1287 1955, Paper presented at WAI 25th Annual Convention, Chicago, IL USA

Year

1955