Description
Experience with the slit strip process for the production of 3/8 inch diameter EC aluminum redraw rod by the Reynolds Metals Co is described. Casting, slitting, redraw rod rolling, thermal operation, and EC rod properties are discussed.
$15.00
Experience with the slit strip process for the production of 3/8 inch diameter EC aluminum redraw rod by the Reynolds Metals Co is described. Casting, slitting, redraw rod rolling, thermal operation, and EC rod properties are discussed.
Experience with the slit strip process for the production of 3/8 inch diameter EC aluminum redraw rod by the Reynolds Metals Co is described. Casting, slitting, redraw rod rolling, thermal operation, and EC rod properties are discussed.
Author(s) | Siltanen, C.W.Reynolds Metals Co. |
---|---|
Publication/Event/Pages | Wire & Wire Products38(11): 1712-1713, 1749-1750 1963, Paper presented at WAI 33rd Annual Convention, Chicago, IL USA |
Year | 1963 |