Tire cord surface analysis by glow discharge spectroscopy

$15.00

The Glow Discharge Spectroscopy (or spectrometry) (GDS), an instantaneous analysis method for determining the chemical composition of a metal surface and interface at the various stages of tire cord production. Simultaneous tracing of concentration depth profiles of up to 16 elements is possible. Considerations, sample testing and results are given.

Description

The Glow Discharge Spectroscopy (or spectrometry) (GDS), an instantaneous analysis method for determining the chemical composition of a metal surface and interface at the various stages of tire cord production. Simultaneous tracing of concentration depth profiles of up to 16 elements is possible. Considerations, sample testing and results are given.